Instruments & Meters

AMiquam Reports 0.1 mm Eddy-Current Detection in LPBF Layers

A sensor built into the recoater scans each freshly deposited layer and maps any indications back onto the part geometry.

Saira QureshiNovember 24, 20265 min read1 views
Concept illustration of a recoater arm carrying an eddy-current sensor across a powder layer, with tiny internal indications marked inside a thin-walled additively manufactured part.

Swiss technology company AMiquam says it has increased the sensitivity of its in-situ eddy current inspection method for metal additive manufacturing, detecting defects as small as 0.1 mm in thin-walled components produced by laser powder bed fusion (LPBF). The results were set out in a technical publication issued ahead of Formnext 2026 and describe inspection during the build rather than relying only on post-build non-destructive testing to establish part quality.

The company frames the work as a way of moving quality assurance closer to the point of manufacture, where defects could be found while a component is still being built.

Sensor carried by the recoater

AMiquam's approach places an eddy current sensor in the recoater assembly of an LPBF machine. As the recoater travels across the build platform, the sensor scans each newly deposited layer and records electromagnetic signals that can indicate internal defects. The inspection data is then mapped onto the component geometry, so that detected anomalies can be located and reported automatically.

0.1 mm indications in a 0.7 mm wall

The most detailed result concerns thin-walled structures of the kind used in additively manufactured heat exchangers. On a 316L stainless steel test specimen with a wall thickness of 0.7 mm, AMiquam reports detecting five artificially introduced holes ranging from 0.1 to 0.5 mm in diameter. Through-holes and blind holes both produced distinct peaks in the eddy current signal, and the company says even the smallest 0.1 mm indication stood out clearly from background signal variation. The measurements were collected across roughly 127 layers, with each hole generating a corresponding peak as the build progressed.

According to the company, the findings point to the possibility of inspecting complex geometries such as triply periodic minimal surface (TPMS) heat exchangers, where internal channels and thin walls make conventional post-process inspection difficult.

An inspection record rather than a certificate

AMiquam also describes a concept for an inspection certificate covering material, layer coverage, detection limits and detected indications, which would give a structured record of inspection data collected during manufacture. The document shown in the publication is an illustrative example and not an actual certification of a component.

Blades: 0.2 mm in the skin, 0.5 mm in the bulk

A second application looks at LPBF-built aeroengine blades, where different laser scanning strategies create distinct microstructures within one part. The blade design uses a conformal scanning strategy in the surface skin and a conventional chessboard strategy in the bulk material. Because these strategies change the microstructure, they also change the eddy current signals recorded during inspection.

AMiquam reports a detection capability of about 0.2 mm within the conformal skin. In the bulk material the threshold is around 0.5 mm, where microstructural variation adds signal fluctuation that makes smaller indications harder to distinguish. The company notes that optimising laser strategies could potentially improve performance in bulk regions.

Locating indications by position and layer

Beyond detection, the technology is intended to establish where a defect sits inside a part. Signals recorded during each recoating pass are mapped to the part geometry, and software automatically identifies indications above predefined thresholds and assigns them X, Y and build-layer coordinates. AMiquam argues this gives manufacturers spatial information rather than a general warning of process instability, which could support later investigations into how a defect arose.

Capturing data throughout a build could also give earlier warning of quality problems instead of revealing them once the part is finished, which the company suggests may matter for aerospace, energy and medical work where qualification and traceability are significant.

Application-specific limits

AMiquam cautions that detection thresholds still depend on component geometry, material and manufacturing parameters, and that the reported figures should be read as application-specific rather than universal performance limits.